Cold_rolling_of_Mg_and_Mg-1Al-0.1Ca.jpg


Summary

Description Pure polycrystalline magnesium failing in a brittle manner already at low deformations, shown here in the rolled state. Pure Mg fractured along macroscopic shear bands when cold rolled to 10% thickness reduction whereas Mg-1Al-0.1Ca could be cold rolled to 54% thickness reduction in several rolling passes of 8% thickness reduction per rolling pass; small sheet sections cut from the rolled sheet after each consecutive rolling pass are presented. Early failure of pure Mg occurs due to the restriction to mainly basal <a> dislocation slip and tensile twinning.
Date
Source https://www.nature.com/articles/s41598-017-10384-0
Author S. Sandlöbes et al
Permission
( Reusing this file )
w:en:Creative Commons
attribution
This file is licensed under the Creative Commons Attribution 4.0 International license.
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.

Captions

Add a one-line explanation of what this file represents

Items portrayed in this file

depicts

image/jpeg

5847aa21a5eb716aa5e4b06322ee193aa445f359

59,883 byte

585 pixel

895 pixel